Chains and Windlasses – 1

There are three major manufacturing Standards that dictate chain dimensions and strengths: ISO Standard (International Standards Organization); NACM Standard (National Assoc. of Chain Manufacturers); Din 766 (Metric Standard). Chain can also be manufactured to no recognized Standard – a questionable choice for use in ground tackle. ISO Standards are used to make chain compatible with…

Read More

Stainless Rust – Part 2

Where deck and above the waterline hull fittings are concerned, brown staining is usually a result of the use of low corrosion resistant 304 or 18-8 stainless alloy and/or exposure to stagnant water.  This alloy is used for 99% of all common fasteners, bolts, screws and nuts.  In the first case, short of replacing the…

Read More

Stainless Steel Rust – Part 1

In some cases rust can be a message.  If the staining is occurring adjacent to stainless steel hardware, then the “rust” is often the byproduct of a process known as crevice corrosion, whereby normally passive, corrosion-resistant stainless steel becomes “active”. “Active” for stainless steel is analogous to rusting for ordinary mild steel.  In both cases, the metal…

Read More

Battery Location versus Inverter Location

Install a fixed-mount inverter no more than 3m from the battery bank, to avoid a voltage drop or extra large cables. Inverters are not ignition protected, so are not safe for installation in compartments with explosive battery gasses; they can be installed in a diesel engine space. In general, pick a location that is cool,…

Read More

Li-ion Battery Capacity Versus Fire Suppression Installation

Fire suppression systems relating to battery installation are usually sized around battery capacity. How much battery capacity largely depends on how it will affect your inverters efficiency delivering the boats onboard loads. Design rule: to be effective, inverters need access to a battery bank that is 20% as large in amp-hours as the inverter size…

Read More

Lithium-ion Fire Best Practice – Part 1

Small electrically powered craft and other vehicles (such as personal watercraft) are becoming more commonly used in place of petrol on yachts. Whilst electric craft do not necessarily represent a greater fire risk than petrol, there are considerable differences in best practice for fire prevention, storage, fire detection and fire suppression when they are stored…

Read More

Crack Propagation – Drill Hole Size

A crack in metal (steel or aluminium) plate or fibreglass matrix can be prevented from spreading (propagating) by drilling a hole at the very end, or just in-front of the crack. The drill hole size does not depend on the length of the crack but the thickness of the plate or matrix. The rule of…

Read More

Twin/Bilge Keel – Potential Failure Points 2

A steel box-section tube was often laminated in the bilge between the keel mouldings. The steel eventually rusts. The outcome of the corrosion process is clear and simple to describe: Iron oxidation (rust) requires four times the volume for its process than the volume of carbon steel it has oxidized. This increase in volume has…

Read More

Twin/Bilge Keel – potential failure points

The moulded integral twin keel construction with ballast inserted from inside relies heavily on the strength of the hull moulding around the root of the keel and the amount of reinforcement on the inside of the hull, in the form of frames, floors and other stiffening. It is therefore important to ensure that the hull…

Read More

Design Rules and Construction Considerations – Part 2

It is generally perceived that transversely framed vessels are easier to build. However, a hull with a parallel mid-body it is relatively easy to fabricate a longitudinally framed mid-body section, since the longitudinals have an easy run in areas of equal width. In the bow and stern areas, where the width measurement decreases rapidly, the…

Read More