Keith Butterfield, Yacht and Marine Surveyor. Costa del Sol, Spain.
A steel box-section tube was often laminated in the bilge between the keel mouldings. The steel eventually rusts. The outcome of the corrosion process is clear and simple to describe: Iron oxidation (rust) requires four times the volume for its process than the volume of carbon steel it has oxidized. This increase in volume has forced the laminate away from the box-section frame.
How the corrosion process initiated is not so straight forward. In 1969 it was widely believed that fibreglass (in older boats almost certainly polyester and chopped matt) was corrosion free and impermeable to water, this subsequently turned out not to be the case. The box-section frame is, for the central section of the hull, fully encapsulated in the resin/fibre matrix. In certain conditions the resin matrix is prone to the passage of water (hydrolysis), and the damp bilge combined with a relatively dry interior of the box-section may have created such conditions. Water reacts with the resin creating a weak galvanic solution. Moisture may have reached the steel section.
Alternatively, the corrosion may be at its worst where the box-section experiences the most compression and tension should flexure of the hull be present, i.e. directly over the bilge keel moulding recess, port and starboard, and in the central section where the two halves of the hull would have moved relative to each other. This continual compression and tension may have fractured the surface of the laminate in the central section or, in the area above the keel, it may have caused stress fracture in the exposed steel, either way it may have allowed the corrosion process to start. The central section itself can have been the site for the accumulation of condensation. Further, the glass fibres themselves are not immune from corrosion. For example, hydrogen gas (perhaps from battery charging) does react in a corrosive way with glass, the result of the process being H2o/water. Any exposed fibres may through wicking have introduced moisture to the steel section. In whatever fashion the corrosion process takes place it is clear damage can be done.