Uncategorised
Engine Mounts
Although they have a very long life expectancy, take a look at the mounts on your main engine or engines as well as those on any other machinery you may have such as water-makers, generators or air conditioning systems. The rubber part of the mount not only acts as a sound and vibration damper but…
Read MoreEngine Zinc Anodes
Often overlooked during maintenance of hull and shaft anodes is the zinc anodes inside the engine block and heat exchangers. The engine zincs, often called pencil zincs, are easy-to-access and remove, they protect the alloy and iron castings of the engine cooling water jacket. The heat exchanger is usually made of a copper alloy and…
Read MoreRe-Boarding Ladder Unassisted
To be certified a boat has to have a way a person can board, or re-board, from the water unassisted. This means most often a folding ladder at the stern. It must be accessible to a person in the water, who can deploy it by themselves without aid. This can be a tall order as…
Read MoreWaves – Deep Troughs
For every high wave, there can also be very deep troughs. There can also be deep troughs without any high wave. There is a real risk of the next wave dropping into the trough and swamping the boat. These troughs do not always come before or after a rogue wave – just a big hole…
Read MoreWave Heights
Chances of a Rogue Wave. There is a growing evidence about extreme waves and their increasing size. The British National Institute of Oceanography calculated 5 meter wave trains using a random process formula – if you take the average height of waves in a wave train, then one wave in 23 will be twice that…
Read MoreTypes of Stainless Steel Corrosion
Crevice Corrosion: a problem with stainless fasteners used in seawater applications where chlorides pit the passivated surface, and low pH salt water attacks the exposed metal. Lacking the oxygen to re-passivate, corrosion continues. As indicated by its name, this corrosion is most common in oxygen restricted crevices, such as under a bolt head. Pitting: Stainless that has…
Read MoreStainless Steel – Staining and Failure
Stainless steel will be from the 300 series and has to be installed and maintained correctly. Type 304 is a good, basic, multipurpose-type; add a bit more nickel content and molybdenum and you get types 316 and 316L, both have improved resistance to corrosion. Type 316L has a lower carbon content to prevent carbide precipitation (and…
Read MoreWhich Anti-Fouling Paint to Choose?
How often you use your boat and how you use it comes into play when deciding on the best paint. Choices for new paint may be limited. Vinyl-based paints can only be applied over vinyl-based paints. Hard paint cannot be applied on ablative (that is, self-polishing) paint. However, ablatives can be painted on top of…
Read MoreAnti-Fouling Aluminium – and Anti-Slime Paints
When painting aluminium hulls or drive units, cuprous oxide isn’t an option, copper on aluminium will set off galvanic corrosion and destroy the metal. When it comes to fiberglass, cuprous oxide is number-one for long-term in-water storage. For those who sail in water with only moderate growth issues, or who put their boat in for…
Read MoreBiocides in Anti-Fouling Paint
TBT tin is the best biocide but is terrible for the environmental – it hasn’t been used for decades. Today, cuprous oxide is the favoured biocide. Effective, but still tough on the environment. The higher the concentration of copper, the more effective — and the more biocides that leech into the water. More environmentally-friendly biocides…
Read More