Keith Butterfield, Yacht and Marine Surveyor. Costa del Sol, Spain.

Modern paints and blast cleaning have reduced the rust problem in steel hulls. Hulls are now all welded and providing good welding practise is used no extra corrosion problems are incurred. A welded seam will rust first because the paint film becomes irregular over the bead. Ground flush, the overlaying paint will give equal protection, and rusting will begin at no particular place.

Paint is mild steels only protection. Most paints prevent rusting by creating an impermeable barrier to galvanic currents. They have high resistance to current flow and prevent galvanic cells. However the success of paint depends upon the thickness of the paint film, surface preparation and painting conditions on the day.

Surface preparation is the most important factor, steel must be clean, dry, free from grease and any other contamination. Painting upon rust seals the ingredients of a galvanic cell and rust will continue to form underneath the paint which will then crack open. Mill scale is the oxide crust formed during manufacture and it is 0.3 volts more noble than the underlying steel. It rapidly pits the paint if not removed before painting. Blast cleaning is common practice and gives a clean surface, hand grinding small areas can give a surface finish as good as blasting. Blast cleaning is generally done to BS4232 otherwise the paint scheme will fail prematurely.

It is essential to apply the paint as soon as possible after cleaning. There is a certain minimum thickness that will ensure success (6-16 mil) depending on the type of paint – several coats are always needed. There are two broad types of paint, ‘conventional’ oil based or the ‘performance’ epoxide, polyurethane/chlorinated type. Providing surface preparation, humidity and temperature conditions are within set limits to avoid water vapour becoming entrapped below the drying paint surface, then success will be probable.