Keith Butterfield, Yacht and Marine Surveyor. Costa del Sol, Spain.
Salt laden environments cause accelerated corrosion damage: 4 basic descriptions relate to each mode.
Described as follows.
‘A’ – The surface is covered in Mill Scale. Mill scale is a thick oxide film formed on steel products after the heat of manufacture once they have been left to cool in air. In steel the oxide is principally magnetic black oxide and is adherent to the surface. In this case it can cover plate but rust has not yet formed.
‘B’ – The mill scale is loose. Loose scale in sheets falls off if the surveyor hits the structure with a test hammer. Loose scale can best be removed by hand or power tool cleaning or a combination of these. It is insignificant/minor corrosion if the extent of corrosion only extends to minor spot rusting and such that an assessment of the corrosion pattern indicates wastage generally not exceeding 30% of the allowable corrosion limits.
‘C’ – Indicates local corrosion at areas with breakdown of the surface or at areas of stress concentration. It is a more active corrosion by atmosphere, moisture or other agents, where chemical or electrochemical attack is visible on the surface. It is a deposit attack under, or around, a local deposit formed on the metal surface in the presence of an electrolyte. It appears as non-protective rust, the rust scale continually breaks off exposing metal to corrosive attack. A little pitting is noticeable. Visual judgement of thickness loss is difficult until serious wastage has occurred.
‘D’ – The pitting corrosion is more evident and produces deep and small diameter pits which may lead to perforation. As it progresses it forms shallow but very wide scabby patches, (e.g. 300mm in diameter). The appearance resembles general corrosion but it may progress to extensive corrosion consisting of hard and/or loose scale, and extensive pitting over 70% or more of the area under consideration, accompanied by evidence of thickness diminution.
Pitting corrosion is easily recognisable as a series of pits on the metal surface, varying from deep cavities of small diameter to relative shallow depressions, pitting corrosion is the most common form of localised attack on the surface of steel alloys. Dirt on a metal surface which is allowed to become wet can be a prime source of pitting attack, a corrosion cell being created by the difference in oxygen concentration between the area under the dirt and surrounding cleaner material. Pitting often stems from the screening effect of silt, scale or corrosion deposits that reduce the oxygen concentration at local points and thus establish differential concentration cells. Corrosion pits often act as initiation sites for more serious forms of corrosion such as intergranular corrosion and fatigue damage, and if allowed to continue untreated can readily perforate thin skins.