Keith Butterfield, Yacht and Marine Surveyor. Costa del Sol, Spain.

During arc-welding hydrogen is released from moisture usually in the coating of the welding electrode. To minimise this low-hydrogen electrodes are used for welding high strength steels. Often pre- and post-heating the metal is applied to allow the hydrogen to diffuse out before it can cause any damage. This is specifically done  with high-strength steels and low alloy steel. Due to the time needed to re-combine hydrogen atoms into the harmful hydrogen molecules, hydrogen cracking can occur up to 24 hours after welding is completed.

For hydrogen induced cracking (HIC) to occur hydrogen needs be present in any flux or other source, it is absorbed by the weld pool and diffuses into the heat affected zone (HAZ) which has a micro-structure susceptible to hydrogen cracking and has cooled to less than 150 centigrade.  HIC in the HAZ is often at the weld toe, but can be under the weld bead or at the weld root. In fillet welds cracks are normally parallel to the weld run but in butt welds cracks can be transverse to the welding direction.

As a result low hydrogen stick electrodes have become the primary electrode for a variety of welding applications. They are ideal for use in applications where base metals have a tendency to crack, where thick sections are to be welded or where the base metal has an alloy content higher than that of mild steel, such as high carbon and low alloy steels. The chemical coating that forms the flux layer is extruded onto the electrode during manufacture, its primary task is to protect the weld pool from nitrogen, oxygen and hydrogen. The electrode coating can also provide alloy and properties to the weld deposit. Low hydrogen electrodes are recommended for three broad areas of application: 1) On steels of poor weldability – low alloy, high carbon, high sulphur, or other steels where cracking can be a problem; 2) when specified by governing codes; 3) for high deposition, out-of-position welds on heavy plate.