Crevice Corrosion: a problem with stainless steel when used in oxygen starved areas where chlorides pit the stainless surfaces and lacking oxygen to ‘re-stainless’ the surface corrosion continues. This corrosion is most common under bolt heads.
Pitting: Stainless that has its protective coating penetrated in a small spot becomes an anodic, while the coated part remains cathodic, causing a pit-type corrosion.
Galvanic Corrosion: Immersing two dissimilar metals in an electrolyte solution (such as seawater) produces an electrical current. The current flows from the anodic metal and toward the cathodic metal, and in the process slowly removes material from the anodic metal.
Intergranular Corrosion: Stainless steel contains a small amount of carbon. When exposed to extremely high temperature (welding, for example) the carbon forces local chrome to form chromium carbide around it, starving the adjacent areas of the chrome it needs for corrosion protection. Choose low carbon stainless such as 304L or 316L when welding.