The paint chosen needs to vary according to the ‘aggressiveness’ of the environment: One of the worst areas is the lower part of the hull just above/on the waterline, which is alternately wetted and dried; impacted by floating objects; berthing procedures; fender abrasion. Corrosion rate increases considerably when steel is not fully immersed but is continually wetted, as in the area between wind and water. Here oxygen is amply provided to hasten any oxidization process afforded by breaks in a protective paint scheme. Just below water line less oxygen is available, however steel can be corroded by the action of organisms close to a muddy bottom or in the top layers of mud and especially in polluted waters. Bacteria use sulphates in the mud water for their metabolism and allow oxygen in the sea water to be made available for the corrosion process. Steel boats lying on mud berths in polluted waters are prone to this sort of attack where the paint has been damaged.
Anode maintenance is important for drying berths where brackish water is encountered, for example river estuaries. Zinc anodes in brackish water form a crust preventing adequate protection. The use of magnesium anodes is a consideration here.