Keith Butterfield, Yacht and Marine Surveyor. Costa del Sol, Spain.

A defect is any flaw that compromises the usefulness of a weld – there are a great variety. Defect causes are: 45% poor process conditions, 32% operator error, 12% wrong technique, 15% incorrect consumables and bad weld grooves. Any defect may result in sudden unexpected failure below the design load or after fewer load cycles than predicted.

Poor Process conditions – To achieve a good quality weld it is essential that the fusion zone extends the full thickness of the work being joined. Good penetration requires the correct balance of heat input and torch traverse speed. Porosity occurs when gases are trapped in the solidifying weld metal. These may arise from damp metal and consumables, or dirt, oil and grease. Consumables need to be stored in dry conditions and work carefully cleaned and degreased. Inclusions occur when several runs are made along a V join using fluxed rods and the slag covering the run is not totally removed before the next pass.

Operator Error – Cracking can occur due to thermal shrinkage or a combination of strain accompanying a phase change. In the case of welded stiff frames, a combination of poor design and inappropriate procedure may result in high residual stress and cracking. To prevent these problems a process of pre-heating and slow controlled post cooling in stages will be required. Factors which increase the risk of cracking include: insufficient weld bead size or inappropriate shape; welding under excessive restraint; material properties – such as a high impurity content or a relatively large shrinkage on solidification. Joint design can have an influence on the level of residual stresses. Large gaps between components will increase the strain on the solidifying weld metal. Weld metal composition is dominated by the filler and as this is usually cleaner than the metal being welded, cracking is less likely with low dilution processes such as MIG. Parent metal composition becomes more important with TIG welding with no filler.

Wrong Technique – Apart from choice of material and filler the main technique for avoiding defects are the control of joint fit-up to reduce gaps. Although the parts to be welded are usually clamped rigidly together it is common for the parts to move as they are heated and cooled. An experienced welder will shim and tack parts in anticipation of their movement. Residual stresses can linger in the welded joints after the continuous weld is made and the clamps removed; therefore, welds are often heat-treated to remove these stresses.

Incorrect Consumables and Poor Groove Preparation – Clean off all contaminants; ensure the welding process will not build up thermal stresses; choose welding parameters with adequate depth to width ratio; choose the correct consumables; avoid high welding speeds (at high current levels); at the run stop, ensure adequate filling of the crater to avoid an unfavourable concave shape.