Hydrogen embrittlement is a form of stress corrosion cracking where hydrogen is the corrosive medium. Some metals are prone to absorbing hydrogen when this gas is present on the surface, subsequently causing cracking. In the context of boat building this relates to high strength steels and some stainless. High tensile steel and non-austentitic hardenable stainless with a yield strength about 1400 N/mm are susceptible. Types 316 and 304 stainless steel (both non-magnetic) are immune.
The mechanism starts with lone hydrogen atoms diffusing through the metal. At high temperatures the elevated solubility of hydrogen allows hydrogen to diffuse into the metal. When these hydrogen atoms re-combine in voids in the metal matrix to form hydrogen molecules, they create pressure from the inside. This pressure can increase to levels where the metal has reduced ductility and tensile strength up to the point where it cracks open (hydrogen induced cracking, HIC). High strength and low alloy steels, nickel and titanium alloys are most susceptible. Hydrogen embrittlement can occur anywhere during manufacturing or in operation where the metal comes into contact with atomic or molecular hydrogen. Processes that can lead to this include cathodic protection, phosphating, pickling and electroplating.